General | ||||
Material Status
|
|
|||
Search for UL Yellow Card
|
|
|||
Availability
|
|
|||
Features
|
|
|||
Uses
|
|
Physical |
Nominal Value
|
Unit
|
Test Method
|
Density / Specific Gravity
|
1.08
|
g/cm3
|
ASTM D792 |
Mechanical |
Nominal Value
|
Unit
|
Test Method
|
Tensile Stress
|
|||
Yield
|
58.0
|
MPa
|
ISO 527-2/50 |
Break, 3.20 mm 1
|
62.8
|
MPa
|
ASTM D638 |
Tensile Elongation
|
|||
Break, 3.20 mm 1
|
10
|
%
|
ASTM D638 |
Break
|
60
|
%
|
ISO 527-2/50 |
Flexural Modulus
|
|||
3.20 mm 2
|
2110
|
MPa
|
ASTM D790 |
-- 3
|
2100
|
MPa
|
ISO 178 |
Flexural Strength
|
|||
3.20 mm 2
|
93.2
|
MPa
|
ASTM D790 |
-- 3
|
85.0
|
MPa
|
ISO 178 |
Impact |
Nominal Value
|
Unit
|
Test Method
|
Charpy Notched Impact Strength
|
ISO 179 | ||
-30°C
|
18
|
kJ/m2
|
|
23°C
|
26
|
kJ/m2
|
|
Notched Izod Impact (23°C, 6.40 mm)
|
200
|
J/m
|
ASTM D256 |
Thermal |
Nominal Value
|
Unit
|
Test Method
|
Deflection Temperature Under Load
|
|||
0.45 MPa, Unannealed
|
160
|
°C
|
ASTM D648 |
0.45 MPa, Unannealed
|
150
|
°C
|
ISO 75-2/Bf |
1.8 MPa, Unannealed
|
135
|
°C
|
ASTM D648 |
Injection |
Nominal Value
|
Unit
|
|
Drying Temperature
|
100 to 120
|
°C
|
|
Drying Time
|
4.0 to 6.0
|
hr
|
|
Rear Temperature
|
260 to 290
|
°C
|
|
Middle Temperature
|
270 to 300
|
°C
|
|
Front Temperature
|
270 to 300
|
°C
|
|
Nozzle Temperature
|
270 to 300
|
°C
|
|
Processing (Melt) Temp
|
260 to 300
|
°C
|
|
Mold Temperature
|
50 to 100
|
°C
|